MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum S7 Tool Steel, UNS T41907  (discontinued **)
Categories: Metal; Ferrous Metal; Tool Steel; Shock-Resisting Steel

Material Notes: An air hardening grade with excellent toughness and suitable for shock resisting service for both hot and cold work tooling applications. Typical uses in blanking, forming and perforating dies, shear blades, chisels, plastic molds, punches, hot gripper and harder dies and hot swaging dies.

Information provided by Allegheny Ludlum

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.76 g/cc0.280 lb/in³literature value
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.50 %0.50 %
Chromium, Cr 3.25 %3.25 %
Iron, Fe 94 %94 %as balance
Manganese, Mn 0.70 %0.70 %
Molybdenum, Mo 1.4 %1.4 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EDRO #7 Shock Resistant S7 Tool Steel
Carpenter S7 Alloy Tool Steel (AISI S7)
Crucible Steel S7 (AISI S7) Tool Steel
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)
Crucible Steel S7 XL (Premium AISI S7) Tool Steel

NLTS7 / 18066

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.