MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crucible Steel S7 (AISI S7) Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Crucible S7 is a shock resisting tool steel with excellent toughness and high strength, along with low to medium wear resistance. It has been widely used for many years to make chisels and punches which undergo shock loading, and has found increasing use for small plastic molds. S7 is easy to machine in the annealed condition and can be readily heat treated. It is deep hardening and in many cases (except for large sections) it can be air quenched, exhibiting minimal distortion on hardening. Due to its relatively high attainable hardness (HRC 58/60) it offers high compressive strength (resistance to deformation) while retaining good toughness. Crucible S7 is a versatile tool steel for both cold and warm shock applications.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 187 - 220187 - 220Annealed
Hardness, Rockwell C 58 - 6058 - 60
Modulus of Elasticity 207 GPa30000 ksi
Charpy Impact 125 J92.2 ft-lbAustenitizing Temperature- 955°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.6 µm/m-°C
@Temperature 20.0 - 205 °C
7.00 µin/in-°F
@Temperature 68.0 - 401 °F
 13.7 µm/m-°C
@Temperature 20.0 - 540 °C
7.61 µin/in-°F
@Temperature 68.0 - 1000 °F
Thermal Conductivity 28.5 W/m-K
@Temperature 95.0 °C
198 BTU-in/hr-ft²-°F
@Temperature 203 °F
Shrinkage -0.100 %
@Temperature 204 °C
-0.100 %
@Temperature 400 °F
Tempered at 400°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.55 %0.55 %
Chromium, Cr 3.25 %3.25 %
Iron, Fe 93.5 %93.5 %As Remainder
Manganese, Mn 0.70 %0.70 %
Molybdenum, Mo 1.4 %1.4 %
Silicon, Si 0.35 %0.35 %
Vanadium, V 0.25 %0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter S7 Alloy Tool Steel (AISI S7)
EDRO #7 Shock Resistant S7 Tool Steel
Crucible Steel S7 XL (Premium AISI S7) Tool Steel
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)

NCRUC024 / 16017

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.