Peroxide Cured, Nitrile Butadiene Rubber (NBR), 55-65 °IRHD. Copolymer of acrylonitrile and butadiene. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600. Applications: Formulation designed for repeated use in equipment associated with the production of foodstuffs intended for human consumption. |