MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: 100% Polystyrene.

Pre-expansion

The unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the smallest EPS beads in the Jackocell® EPS grade selection.

Shape Moulding

The unique design of polystyrene chains in combination with small beads and narrow bead size distribution adds numerous advantages to Jackocell® R411 in shape moulding. Fast moulding cycles, good fusion and h eat resistance - and easy to reach good surface. The additional broad moulding window further reduces waste material and maintains high quality to the extent that it can be recognized long term on productivity and financial earnings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0160 g/cc0.000578 lb/in³2 minute residence time pre-expander
 0.0180 g/cc0.000650 lb/in³2.4 minute residence time pre-expander
 0.0210 g/cc0.000759 lb/in³1 minute residence time pre-expander
 0.0330 g/cc0.00119 lb/in³0.5 minute residence time pre-expander
Water Absorption 4.0 %4.0 %13-20 hour silo ageing time; Volume%
Bead Size 0.400 - 0.700 mm0.0157 - 0.0276 in
 
Chemical PropertiesMetricEnglishComments
Blowing Agent Content >= 6.0 %>= 6.0 %Pentane
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 0.365 MPa52.9 psi16 hour silo aging time, 20 kg/m^3
 0.368 MPa53.4 psi64 hours silo aging time, 20 kg/m^3
 0.369 MPa53.5 psi48 hour silo aging time, 20 kg/m^3
 0.370 MPa53.7 psi32 hour silo aging time, 20 kg/m^3
Compressive Strength 1.37 MPa199 psi16 hour silo aging time, 20 kg/m^3
 1.39 MPa202 psi32 hour silo aging time, 20 kg/m^3
 1.39 MPa202 psi48 hour silo aging time, 20 kg/m^3
 1.39 MPa202 psi64 hours silo aging time, 20 kg/m^3
 
Descriptive Properties
Coefficient of Variation (%), max12
Molding Cycle Time (sec)10048 hour silo aging time, 20 kg/m^3
 13032 hour silo aging time, 20 kg/m^3
 1756 hour silo aging time, 20 kg/m^3
 9064 hours silo aging time, 20 kg/m^3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding
IRPC Polimaxx Pentfoam 455E Expandable Polystyrene
NOVA Chemicals Dytherm® 340R Expandable Polystyrene

PJACK003 / 85569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.