Nitrile Butadiene Rubber, 45-55 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class B, approval ref.: 67/6.11.iv. MSL lab code 1.R. Also meets British Standard BS2494 Type G. Applications: Elastomeric seals for use in pipelines carrying manufactured or natural gas at operating temperatures of -5° to +40°C and pressures up to 7 bar. |