MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: LF320 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It was developed for cast film extrusion. Films obtained with this product show a good processing performance balanced with good optical and mechanical properties as well as processability. It has a very low gel amount. It contains processing aid and antioxidant additives. Its applications include: stretch films, liners, LDPE and HDPE blends, and packages for general use. Recommended processing conditions for film extrusion are about 170 - 210 ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM-D1505
Melt Flow 2.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 1090 %1090 %ASTM-D882
Film Elongation at Break, TD 1380 %1380 %ASTM-D882
Elmendorf Tear Strength MD 60 g60 gASTM-D1922
Elmendorf Tear Strength TD 320 g320 gASTM-D1922
Elmendorf Tear Strength, MD 1.58 g/micron40.1 g/milASTM-D1922
Elmendorf Tear Strength, TD 8.42 g/micron214 g/milASTM-D1922
Dart Drop 1.58 g/micron40.1 g/milASTM-D1709
Dart Drop Test 60.0 g0.132 lbASTM-D1709
Film Tensile Strength at Break, MD 30.0 MPa4350 psiASTM-D882
Film Tensile Strength at Break, TD 20.0 MPa2900 psiASTM-D882
1% Secant Modulus, MD 180 MPa26100 psiASTM-D882
1% Secant Modulus, TD 230 MPa33400 psiASTM-D882
 
Optical PropertiesMetricEnglishComments
Haze 23 %23 %ASTM-D1003
Gloss 68 %68 %Angle 60°; ASTM-D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Flexirene® MR 50 U Linear Low Density Polyethylene
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene
Borealis Borstar® FB2310 LLDPE for Film
Baystar™ Lumicene® mPE M 3410 EP Metallocene Medium Density Polyethylene Film Resin
Braskem LL6801N LLDPE Blown Film Extrusion Polyethylene Copolymer

PBRAS868 / 106714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.