MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Baystar™ Lumicene® mPE M 3410 EP Metallocene Medium Density Polyethylene Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: Characteristics:
  • Outstanding clarity and gloss
  • Excellent bubble stability
  • High stiffness
  • Good tear strength
  • Good puncture resistance
  • Good heat sealing properties
  • Excellent compatibility with LDPE and LLDPE
Applications:
  • Tissue and towel overwrap films
  • Clarity shrink films
  • Protective packaging
  • Food packaging
  • Laminations and multilayer packaging films
  • Machine direction oriented (MDO) films
Film was produced at 1.0 mil with a 2.5:1 BUR.

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture in the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.934 g/cc0.0337 lb/in³ASTM D-792
Water Vapor Transmission 10.1 g/m²/day0.650 g/100 in²/day100°F / 90%RH; ASTM F-1294
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
High Load Melt Index 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
30 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 400 %400 %ASTM D-882, A
Film Elongation at Break, TD 650 %650 %ASTM D-882, A
Elmendorf Tear Strength MD 55 g55 gASTM D1922
Elmendorf Tear Strength TD 400 g400 gASTM D1922
Dart Drop Test 60.0 g0.132 lbASTM D1709, A
Film Tensile Strength at Break, MD 44.1 MPa6400 psiASTM D-882, A
Film Tensile Strength at Break, TD 42.1 MPa6100 psiASTM D-882, A
1% Secant Modulus, MD 365 MPa53000 psiASTM D-882, A
1% Secant Modulus, TD 386 MPa56000 psiASTM D-882, A
 
Thermal PropertiesMetricEnglishComments
Melting Point 124 °C255 °FASTM D-3417
 
Optical PropertiesMetricEnglishComments
Haze 9.00 %9.00 %ASTM D1003
Gloss 65 %65 %45°; ASTM D 2457
 
Descriptive Properties
Food StatusFormulated to comply with most requirements of food packaging regulations

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding
Total Lumicene® mPE M5220 M Metallocene High Density Polyethylene
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene

PBAYST910 / 38667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.