MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ex-Tech Plastics VersaTech™ PET Ex-Alloy 3400, 100% Post Consumer FDA, RPET Extruded Sheet
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Delivering all the qualities of PET, this sheet is developed using post consumer material, allowing the packaging to carry marketing reference terms such as sustainability, green and recycled.

Characteristics:
Transparent
High impact
Tear resistant

End Uses:
Consumer packaging: clamshell, blister, tray

Information provided by Ex-Tech Plastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Test 75 - 81 cm³/g0.75 - 0.81 dl/gIntrinsic Viscosity
 
Thermal PropertiesMetricEnglishComments
Melting Point 243 - 249 °C469 - 480 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
CIE Color<7.2b
 >69.0L
 -2.0 to -3.0a

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)
Chase Plastics CP Pryme® PC300RHF Polycarbonate, Recycled Content
Ex-Tech Plastics VersaTech™ APET
Ex-Tech Plastics VersaTech™ RPET Packaging Polymer

PEXTEC991 / 133216

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.