MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ex-Tech Plastics VersaTech™ RPET Packaging Polymer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Primarily used for consumer packaging, VersaTech RPET delivers on excellent clarity and high gloss, while providing good impact and tear resistance properties that are demanded in today’s retail environment.

Characteristics:
Excellent clarity
Impact and tear resistant
High gloss

End Uses:
Consumer packaging

Information provided by Ex-Tech Plastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
Viscosity Measurement >= 0.65>= 0.65Intrinsic Viscosity; ASTM D3835
Linear Mold Shrinkage 0.020 - 0.050 cm/cm0.020 - 0.050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 48.26 - 55.16 MPa7000 - 8000 psiASTM D638
Elongation at Break 100 - 200 %100 - 200 %
Flexural Modulus 2.07 - 2.41 GPa300 - 350 ksiASTM D790
 
Optical PropertiesMetricEnglishComments
Haze <= 10 %
@Thickness <=0.508 mm
<= 10 %
@Thickness <=0.0200 in
ASTM D1003
Transmission, Visible >= 85 %>= 85 %ASTM D1003
 
Descriptive Properties
Clarity>97%ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ex-Tech Plastics VersaTech™ APET
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Spartech APET SP4110 Copolyester Sheet
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
Bamberger Polymers Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade

PEXTEC990 / 133215

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.