MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® 473 Polyester Film, 200 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 473 is a high clarity polyester film manufactured with a coating on one surface that improves slip and handling characteristics. The opposite surface is raw polyester (non-coated). The slip treated surface is wound inside of the roll and the raw surface (non-coated) is on the outside surface of the roll.

Typical Applications: Melinex 473 is used in many general industrial applications where clarity and handling properties are critical, e.g., overlay, lamination and printing applications.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD >= 89.6 MPa>= 13000 psiASTM D882A
Film Tensile Strength at Yield, TD >= 89.6 MPa>= 13000 psiASTM D882A
Coefficient of Friction, Dynamic <= 0.70<= 0.70A-B; ASTM D1894
Film Tensile Strength at Break, MD >= 172 MPa>= 25000 psiASTM D882A
Film Tensile Strength at Break, TD >= 172 MPa>= 25000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 2.5 %
@Temperature 190 °C,
Time 300 sec
2.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
1.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
 
Descriptive Properties
Yield (nominal)9918 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 461 Polyester Film
DuPont Teijin Films Melinex® 513P Polyester Film, 650 Gauge
DuPont Teijin Films Melinex® 505 Polyester Film
DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 478 Polyester Film, 200 Gauge

PDTZ9117 / 139492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.