MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® 505 Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 505 is a high clarity polyester film which is pretreated on both sides to promote adhesion to most industrial coating and inks.

Approvals: UL 94 VTM-2 - for 1000 gauge (0.26mm) only

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 96.5 MPa14000 psiASTM D882A
Film Tensile Strength at Yield, TD 96.5 MPa14000 psiASTM D882A
Film Elongation at Break, MD 180 %180 %ASTM D882A
Film Elongation at Break, TD 105 %105 %ASTM D882A
Coefficient of Friction, Static 0.500.50ASTM D1894
Film Tensile Strength at Break, MD 179 MPa26000 psiASTM D882A
Film Tensile Strength at Break, TD 228 MPa33000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 2.5 %
@Temperature 190 °C,
Time 300 sec
2.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
1.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze  0.30 %
@Thickness 0.0762 mm
0.30 %
@Thickness 0.00300 in
ASTM D1003
 0.30 %
@Thickness 0.102 mm
0.30 %
@Thickness 0.00400 in
ASTM D1003
 0.40 %
@Thickness 0.127 mm
0.40 %
@Thickness 0.00500 in
ASTM D1003
 0.50 %
@Thickness 0.165 mm
0.50 %
@Thickness 0.00650 in
ASTM D1003
 0.60 %
@Thickness 0.178 mm
0.60 %
@Thickness 0.00700 in
ASTM D1003
Transmission, Visible  87 %
@Thickness 0.178 mm
87 %
@Thickness 0.00700 in
TLT; ASTM D1003
 87.2 %
@Thickness 0.165 mm
87.2 %
@Thickness 0.00650 in
TLT; ASTM D1003
 88 %
@Thickness 0.127 mm
88 %
@Thickness 0.00500 in
TLT; ASTM D1003
 88.3 %
@Thickness 0.102 mm
88.3 %
@Thickness 0.00400 in
TLT; ASTM D1003
 88.5 %
@Thickness 0.0762 mm
88.5 %
@Thickness 0.00300 in
TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 461 Polyester Film
DuPont Teijin Films Melinex® 515 Polyester Film
DuPont Teijin Films Melinex® 514P Polyester Film
DuPont Teijin Films Melinex® 513P Polyester Film, 650 Gauge
DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge

PDTZ9121 / 139496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.