MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual Mg surface treatments may be applied. Uses include motorsports and aerospace.

Key Words: UNS M12310; AMS 4429
Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.82 g/cc0.0658 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 65 - 7565 - 75
Tensile Strength >= 248 MPa>= 36000 psiMinimum design value
 179 MPa
@Temperature 260 °C
26000 psi
@Temperature 500 °F
Typical
 241 MPa
@Temperature 191 °C
35000 psi
@Temperature 375 °F
Typical
 262 MPa
@Temperature 121 °C
38000 psi
@Temperature 250 °F
Typical
 270 MPa
@Temperature -35.0 °C
39200 psi
@Temperature -31.0 °F
Typical
 280 MPa
@Temperature 22.2 °C
40600 psi
@Temperature 72.0 °F
Tensile Strength, Yield  145 MPa
@Strain 0.2 %,
Temperature 260 °C
21000 psi
@Strain 0.2 %,
Temperature 500 °F
Typical
 >= 145 MPa
@Strain 0.2 %,
Temperature 22.2 °C
>= 21000 psi
@Strain 0.2 %,
Temperature 72.0 °F
Minimum design value
 159 MPa
@Strain 0.2 %,
Temperature 191 °C
23000 psi
@Strain 0.2 %,
Temperature 375 °F
Typical
 165 MPa
@Strain 0.2 %,
Temperature 121 °C
24000 psi
@Strain 0.2 %,
Temperature 250 °F
Typical
 170 MPa
@Strain 0.2 %,
Temperature 22.2 °C
24700 psi
@Strain 0.2 %,
Temperature 72.0 °F
Typical
Elongation at Break >= 2.0 %>= 2.0 %Minimum design value
 5.0 %5.0 %Typical
 7.0 %
@Temperature -35.0 °C
7.0 %
@Temperature -31.0 °F
Typical
Creep Strength  82.7 MPa
@Temperature 204 °C,
Time 1.98e+6 sec
12000 psi
@Temperature 400 °F,
Time 550 hour
0.1% creep strain
 96.5 MPa
@Temperature 204 °C,
Time 360000 sec
14000 psi
@Temperature 400 °F,
Time 100 hour
0.1% creep strain
 117 MPa
@Temperature 204 °C,
Time 234000 sec
17000 psi
@Temperature 400 °F,
Time 65.0 hour
0.1% creep strain
Modulus of Elasticity 44.1 GPa6400 ksi
Compressive Yield Strength 168 MPa
@Strain 0.2 %
24400 psi
@Strain 0.2 %
Typical
Compressive Strength 367 MPa53200 psiTypical
Poissons Ratio 0.270.27
Fatigue Strength 115 - 120 MPa
@# of Cycles 5.00e+7
16700 - 17400 psi
@# of Cycles 5.00e+7
Push-Pull; R = 0.1
Fracture Toughness 14.9 MPa-m½13.6 ksi-in½KIC
Shear Modulus 17.4 GPa2520 ksiCalculated
Shear Strength 172 MPa25000 psi
Charpy Impact 1.7 J
@Temperature -35.0 °C
1.3 ft-lb
@Temperature -31.0 °F
Notched
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000946 ohm-cm0.00000946 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 26.6 µm/m-°C14.8 µin/in-°F
Specific Heat Capacity 1.00 J/g-°C0.240 BTU/lb-°F
Thermal Conductivity 116 W/m-K804 BTU-in/hr-ft²-°F
Melting Point 545.0 - 640.0 °C1013 - 1184 °F
Solidus 545.0 °C1013 °F
Liquidus 640.0 °C1184 °F
Maximum Service Temperature, Air 204 °C400 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 520 °C
@Time 28800 sec
968 °F
@Time 8.00 hour
Follow with hot quench and aging
Aging Temperature 200 °C
@Time 57600 sec
392 °F
@Time 16.0 hour
Follow with air cool
 
Component Elements PropertiesMetricEnglishComments
Gadolinium, Gd 1.0 - 1.7 %1.0 - 1.7 %
Magnesium, Mg 94.7 - 96.2 %94.7 - 96.2 %as balance; includes saturation of Zr
Neodymium, Nd 2.6 - 3.1 %2.6 - 3.1 %
Zinc, Zn 0.20 - 0.50 %0.20 - 0.50 %
 
Descriptive Properties
Corrosion Resistance10 - 30 mpyASTM B117 salt spray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Magnesium Alloy
Magnesium Elektron Elektron® AZ31B Magnesium Extrusion Alloy, UNS M11311
Magnesium, Mg; Annealed Sheet
Magnesium, Mg; Hard-Rolled Sheet
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia

NMAGEL898 / 147647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.