MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kostat BK-STAT P048BK PP Sheet
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness requirements in comparison to other materials based on Hygroscopic Antistats, Inherently Conductive Polymer Coating, or Conductive Fillers such as carbon fibers and carbon blacks.

BK-STAT Compounds exhibit superior property and processing characteristics compared with other competitive IDP based compounds.

Special Features:

  • Superior Permanent Static Dissipation
  • Excellent Wear Resistance
  • Humidity Insensitivity
  • Exceptionally High Impact Resistance
  • No Particle Generation
  • Excellent Processibility

Applications:

  • Semiconductor Packaging
  • LCD Packaging
  • Electrical & Electronics
  • Medical Devices
  • Storage Disks
  • Appliances
  • Consumer Goods
  • Clean Room Accessories

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+9 - 1.00e+11 ohm1.00e+9 - 1.00e+11 ohmASTM D257
Static Decay <= 0.50 sec<= 0.50 sec5kV to 50V; FTMS 101C
 
Processing PropertiesMetricEnglishComments
Drying Temperature 60.0 - 70.0 °C140 - 158 °F
Dry Time 3 - 4 hour3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EXT 399 X 113653 SSC-64013 Polycarbonate (PC) Sheet Product - Glow in the Dark
Kostat ICP-STAT ICS-1002 PP Sheet
PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene
RTP Company RTP 227 H SI 2 Z Nylon 6/6 (PA); Mineral - Impact Modified - Silicone Lubricated - FDA Compliant Ingredients - Preliminary Data Sheet
Versalis EDISTIR PD RK4122H High Impact Polystyrene (HIPS)

PKOSTAT04 / 49039

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.