MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kostat ICP-STAT ICS-1002 PP Sheet
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials based on Hygroscopic Antistats and Conductive Fillers. This product exhibits superior transparency and clarity.

Special Features:

  • Superior Permanent Static Dissipation
  • Humidity Insensitivity
  • Excellent Wear resistance
  • Low Particle Generation
  • Superior Transparency and Clarity
  • Low Ionic Contamination
  • Excellent Chemical Resistance with Environmentally Friendly Materials

Applications:

  • Semiconductors Packaging
  • LCD Components Packaging
  • HDD Components Packaging
  • Electrical & Electronics Packaging
  • Medical Devices Packaging
  • Clean Room Accessories

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.3 MPa4400 psiASTM D638
Flexural Strength 37.9 MPa5500 psiASTM D790
Flexural Modulus 1.14 GPa165 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1e+05 - 1.00e+6 ohm1e+05 - 1.00e+6 ohmASTM D257
 1.00e+6 ohm1.00e+6 ohmafter 100% elongation; ASTM D257
 1.00e+7 ohm1.00e+7 ohmafter 200% elongation; ASTM D257
 1.00e+9 ohm1.00e+9 ohmafter 250% elongation; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C130 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 85 %>= 85 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EXT 399 X 113653 SSC-64013 Polycarbonate (PC) Sheet Product - Glow in the Dark
Kostat BK-STAT P048BK PP Sheet
Versalis EDISTIR PD RK4122H High Impact Polystyrene (HIPS)
RTP Company RTP 227 H SI 2 Z Nylon 6/6 (PA); Mineral - Impact Modified - Silicone Lubricated - FDA Compliant Ingredients - Preliminary Data Sheet
RTP Company EMI 861.3 Acetal (POM) Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - (Preliminary Data Sheet)

PKOSTAT08 / 49043

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.