MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ CCM605 PTFE, 25% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Type II, free flowing.

Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.24 g/cc2.24 g/ccASTM D4894
Bulk Density 0.710 g/cc0.0257 lb/in³ASTM D4894
Particle Size 750 µm750 µmASTM D4894
Deformation 1.0 %
@Pressure 15.00 MPa
1.0 %
@Pressure 2175 psi
permanent; ASTM D621
 2.0 %
@Time 86400 sec,
Pressure 15.00 MPa
2.0 %
@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262Initial; ASTM D2240
 57
@Time 15.0 sec
57
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 15.2 MPa2200 psiASTM D4894
Elongation at Break 300 %300 %ASTM D4894
Tensile Modulus 0.165 GPa24.0 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
CTE, linear  73.8 µm/m-°C
@Temperature 30.0 - 100 °C
41.0 µin/in-°F
@Temperature 86.0 - 212 °F
ASTM E831
 91.8 µm/m-°C
@Temperature 100 - 200 °C
51.0 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
 140 µm/m-°C
@Temperature 200 - 300 °C
78.0 µin/in-°F
@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity  0.240 W/m-K
@Temperature 100 °C
1.67 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1530
 0.260 W/m-K
@Temperature 250 °C
1.80 BTU-in/hr-ft²-°F
@Temperature 482 °F
ASTM E1530
Shrinkage 2.8 %2.8 %ASTM D4894

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler
3M Dyneon™ TFM™ 1700 PTFE
3M Dyneon™ TFM™ 1700 Modified PTFE Powder
3M Dyneon™ TF 5050Z PTFE

PDYL9980 / 129998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.