MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ CCM605 PTFE, 25% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Type II, free flowing.

Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.24 g/ccASTM D4894
Bulk Density 0.710 g/ccASTM D4894
Particle Size 750 µmASTM D4894
Deformation 1.0 %
@Pressure 15.00 MPa
permanent; ASTM D621
 2.0 %
@Time 86400 sec,
Pressure 15.00 MPa
ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62Initial; ASTM D2240
 57
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 15.2 MPaASTM D4894
Elongation at Break 300 %ASTM D4894
Tensile Modulus 24000 psiASTM D638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.0 µin/in-°F
@Temperature 30.0 - 100 °C
ASTM E831
 51.0 µin/in-°F
@Temperature 100 - 200 °C
ASTM E831
 78.0 µin/in-°F
@Temperature 200 - 300 °C
ASTM E831
Thermal Conductivity 0.240 W/m-K
@Temperature 100 °C
ASTM E1530
 0.260 W/m-K
@Temperature 250 °C
ASTM E1530
Shrinkage 2.8 %ASTM D4894

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler
3M Dyneon™ TFM™ 1700 PTFE
3M Dyneon™ TFM™ 1700 Modified PTFE Powder
3M Dyneon™ TF 5050Z PTFE

PDYL9980 / 129998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.