MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene with 20% Glass Fiber Filler

Material Notes:

Information provided by PolyPlastic Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inISO 294-4
Melt Flow 0.50 - 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.50 - 1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 52.0 MPa7540 psiISO 5272
Elongation at Break 7.5 %7.5 %ISO 527
Flexural Strength 75.0 MPa10900 psiISO 178
Flexural Modulus 3.20 GPa464 ksiISO 178
Charpy Impact Unnotched  5.00 J/cm²
@Temperature -40.0 °C
23.8 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 6.50 J/cm²
@Temperature 20.0 °C
30.9 ft-lb/in²
@Temperature 68.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -40.0 °C
4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 2.20 J/cm²
@Temperature 20.0 °C
10.5 ft-lb/in²
@Temperature 68.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 29.0 µm/m-°C16.1 µin/in-°FISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 112 °C234 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 145 °C293 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber
EPICHEM Epilen PP 20GF NAT Polypropylene, 20% Glass Fiber
Techmer ES HiFill® PP GF15 CC 15% Glass Filled
GEHR Plastics PP-30GF Polypropylene, 30% Glass Fiber
Polyplastic Armlen® PP GF MF 30-1 Polypropylene, 30% Glass and Mineral Filled

PPOLYP924 / 157151

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.