MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastic Armlen® PP GF MF 30-1 Polypropylene, 30% Glass and Mineral Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Glass/Mineral Reinforced

Material Notes: Injection molding

Information provided by PolyPlastic Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.0080 cm/cm0.0070 - 0.0080 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.0080 cm/cm0.0070 - 0.0080 in/inISO 294-4
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 30 %30 %ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 69.0 MPa10000 psiISO 527
Flexural Strength 85.0 MPa12300 psiISO 178
Flexural Modulus 3.64 GPa528 ksiISO 178
Charpy Impact Unnotched 4.10 J/cm²
@Temperature 23.0 °C
19.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 156 °C313 °FISO 75B
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 240 °C446 - 464 °F
Mold Temperature 60.0 °C140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black
Techmer ES HiFill® PP GF15 CC 15% Glass Filled
Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber
Polyplastic Armlen® PP GF 30-5HS-901 Polypropylene, 30% Glass Filled
Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber

PPOLYP912 / 157139

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.