MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Haysite Heatmeiser® Composite Thermal Insulation
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: A thermal insulation sheet, Heatmeiser® is a specially engineered composite offering superior energy efficiency, temperature control and durability for high temperature mold jacket and platen thermal insulation applications. Heatmeiser thermal conductivity results separate this material from all other glass reinforced products. Available is thicknesses from 1/8" - 2.00". Color - Lt. Gray.

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.25 %0.25 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 141 MPa20500 psiASTM D790
Compressive Strength  124 MPa
@Temperature 149 °C
18000 psi
@Temperature 300 °F
ASTM D695
 131 MPa
@Temperature 204 °C
19000 psi
@Temperature 400 °F
ASTM D695
 133 MPa
@Temperature 260 °C
19300 psi
@Temperature 500 °F
ASTM D695
Izod Impact, Notched 4.81 J/cm9.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.1 µm/m-°C11.7 µin/in-°FASTM D696
Thermal Conductivity 1.20 W/m-K8.33 BTU-in/hr-ft²-°FASTM D177
Maximum Service Temperature, Inert 288 °C550 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silres® BS 1042 Silicone Masonry Water Repellent
Wool Cloth Fiber
Phillips 66 Wool Processing Oil ISO Grade 22
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket

PHAY510 / 142466

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.