MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Wool Processing Oil ISO Grade 22
Categories: Fluid; Lubricant

Material Notes: Wool Processing Oil is a high-quality, low-viscosity mineral oil developed for use as a wool processing oil. It improves cohesion of the wool fibers and helps protect them during processing and spinning the wool into yarn. It also helps reduce static during processing. Wool Processing Oil has very light color and is nonstaining. It is inhibited against oxidation to maintain color stability

Applications:

  • Wool processing
Features/Benefits:
  • Very light color
  • Nonstaining
  • Good color stability

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.853 g/cc0.853 g/cc
Density 0.851 g/cc0.0307 lb/in³
Viscosity Measurement 102102Index
Saybolt Viscosity at 100°F 108.5 SUS108.5 SUS
Saybolt Viscosity at 210°F 40.8 SUS40.8 SUS
Kinematic Viscosity at 40°C (104°F) 22.5 cSt22.5 cSt
Kinematic Viscosity at 100°C (212°F) 4.4 cSt4.4 cSt
ASTM Color 0.500.50ASTM D1500
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Flash Point 209 °C408 °FCOC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silres® BS 1042 Silicone Masonry Water Repellent
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket
Microtherm Group Super A Alumina Based Thermal Insulation
Microtherm Group Board Filament Reinforced Pyrogenic Silica Thermal Insulation

WCON5260 / 198513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.