MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Park Aerospace Nelcote® E-765 Epoxy Prepreg, T700 12K 2x2 Twill Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request.

Key Features and Benefits:

  • Designed to replace first generation 350°F (176°C) cure systems.
  • Wide cure temperature process window of 250°F to 350°F
  • Exhibits very low void content, i.e., <2% after vacuum cure.
  • Superior fiber property translation.
  • 180°F Wet service temperature after ~250°F cure
  • Good tack and drape characteristics for 3 weeks at room temperature

Applications/Qualifications:

  • Primary Aircraft Structures
    • Fuselage
    • Wing
    • Control Surfaces
  • Secondary Aircraft Structures
    • Aircraft Frames
    • Doors
    • Shelves
    • Bulkheads

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.5 %<= 1.5 %
Thickness 381 microns15.0 milcured, per ply
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 841 MPa
@Temperature 21.1 °C
122000 psi
@Temperature 70.0 °F
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95
Tensile Modulus 57.9 GPa
@Temperature 21.1 °C
8400 ksi
@Temperature 70.0 °F
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95
Compressive Strength 738 MPa
@Temperature 21.1 °C
107000 psi
@Temperature 70.0 °F
Dry; Vacuum/Oven Cured; SACMA 1-94
Compressive Modulus 55.8 GPa
@Temperature 21.1 °C
8100 ksi
@Temperature 70.0 °F
Dry; Vacuum/Oven Cured; SACMA 1-94
Shear Strength 60.7 MPa
@Temperature 21.1 °C
8800 psi
@Temperature 70.0 °F
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 165 °C329 °FDry; DMA
 
Processing PropertiesMetricEnglishComments
Gel Time 2.00 - 6.00 min
@Temperature 135 °C
2.00 - 6.00 min
@Temperature 275 °F
Shelf Life 6.00 Month
@Temperature -17.8 °C
6.00 Month
@Temperature 0.000 °F
 
Descriptive Properties
Fabric Area Weight (g/m²)370
Prepreg Resin Content (%)37-43
Resin Flow (%)12-24275°F, 15psi
TackLight-Medium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay EF1812 Polycarbosilane Polymer, Pyrolized with T300 Carbon Fabric
Solvay LTM® 26EL Epoxy with T300 Woven Carbon Fiber Laminate
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced

PPARK035 / 89307

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.