MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Buna FX 3234A HM Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Buna FX 3234A-2 is a functionalized high styrene SSBR designed to improve the polymer to filler interaction with the silica filler inside the tread compound. This reduces the hysteresis inside the tread compound thus reducing the rolling resistance of the tire. Traction indicators have also been improved. The product has a Mooney Viscosity of 80 after the addition of the 37.5 phr of TDAE oil which is in compliance with the European directive 2005/69/ec.

CAS No: 9003-17-2

Plant: PT. Jerome

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %MO AQ 255 LAB
Mooney Viscosity 8080[ME]; ASTM D1645
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month
@Temperature <=35.0 °C
24.0 Month
@Temperature <=95.0 °F
 
Descriptive Properties
Content27.3 percentOil, MO AQ 246 LAB
 32 percentvinyl, MO AQ 254 LAB
 34 percentStyrene, MO AQ 243 LAB (UV)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 32341 Phenolic Resin
Sumitomo Bakelite Durez® 32340 Phenolic Resin
Rogers Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Misumi Z3234 Chromium Copper
ChevronTexaco Vistac® ISO 32 Rock Drill Oil

PLANY8505 / 208898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.