MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the melt strength ideally suited for blow molding and other applications requiring ultra high melt viscosity. It exhibits improved strength, stiffness and creep resistance compare to standard blow molding grades. Outstanding permeability and chemical resistance to oils, hydrocarbons and most solvents are other advantages along with excellent stiffness ad the ability to fabricate complex shapes for cost effective metal replacements.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³dry; ISO 1183
Water Absorption 1.4 %1.4 %24 hour; ISO Test
 8.3 %8.3 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.3 %2.3 %beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi0.2 in/min; ASTM Test
 25.0 MPa
@Temperature 120 °C
3630 psi
@Temperature 248 °F
ISO Data
 25.0 MPa
@Temperature 120 °C
3630 psi
@Temperature 248 °F
ASTM Test
 40.0 MPa
@Temperature 80.0 °C
5800 psi
@Temperature 176 °F
ASTM Test
 40.0 MPa
@Temperature 80.0 °C
5800 psi
@Temperature 176 °F
ISO Data
 110 MPa
@Temperature -40.0 °C
16000 psi
@Temperature -40.0 °F
ASTM Test
 110 MPa
@Temperature -40.0 °C
16000 psi
@Temperature -40.0 °F
ISO Data
Tensile Strength, Ultimate 60.0 MPa8700 psi5mm/min; ISO 527
Tensile Strength, Yield 65.0 MPa9430 psi50mm/min; ISO 527
 65.0 MPa9430 psi2 in/min; ASTM Test
Elongation at Break 20 %20 %50mm/min, Nominal strain; ISO 527
 30 %30 %2 in/min; ASTM Test
 2.0 %
@Temperature -40.0 °C
2.0 %
@Temperature -40.0 °F
ASTM Test
 2.0 %
@Temperature -40.0 °C
2.0 %
@Temperature -40.0 °F
ISO Data
 20 %
@Temperature 120 °C
20 %
@Temperature 248 °F
ISO Data
 20 %
@Temperature 120 °C
20 %
@Temperature 248 °F
ASTM Test
 30 %
@Temperature 80.0 °C
30 %
@Temperature 176 °F
ASTM Test
 30 %
@Temperature 80.0 °C
30 %
@Temperature 176 °F
ISO Data
Elongation at Yield 15 %15 %50mm/min; ISO 527
 15 %15 %2 in/min; ASTM Test
Tensile Modulus 3.10 GPa450 ksi1mm/min; ISO 527
 1.50 GPa
@Temperature 120 °C
218 ksi
@Temperature 248 °F
ISO Data
 1.90 GPa
@Temperature 80.0 °C
276 ksi
@Temperature 176 °F
ISO Data
 6.40 GPa
@Temperature -40.0 °C
928 ksi
@Temperature -40.0 °F
ISO Data
Flexural Strength 80.0 MPa11600 psiASTM Test
 265 MPa
@Temperature -40.0 °C
38400 psi
@Temperature -40.0 °F
ASTM Test
Flexural Modulus 1.97 GPa286 ksiASTM Test
Izod Impact, Notched 0.400 J/cm
@Temperature -40.0 °C
0.749 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 1.55 J/cm
@Thickness 3.17 mm
2.90 ft-lb/in
@Thickness 0.125 in
ASTM Test
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 95.0 °C203 °FInjection molding
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueBlow Molding
ProcessingBlow molding
 Injection Molding
Special characteristicHeat stabilized or stable to heat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry)
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry)
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
BASF Ultramid® 8202C PA6 (Dry)

PBASF9198 / 84962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.