MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating parts

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.32 g/cc0.0477 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.1 - 2.5 %2.1 - 2.5 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 6.8 - 7.4 %6.8 - 7.4 %ISO 62
Viscosity Measurement 140140ISO 307
Linear Mold Shrinkage 0.0035 cm/cm0.0035 in/inrestricted
Melt Flow 72.6 g/10 min
@Load 5.00 kg,
Temperature 275 °C
72.6 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 105 MPa15200 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 8.5 %8.5 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 5.50 GPa798 ksiISO 527-1/-2
Flexural Strength 150 MPa21800 psiat max force; ISO 178
Flexural Modulus 4.20 GPa609 ksiISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 10.5 J/cm²
@Temperature 23.0 °C
50.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 3000 MPa
@Strain <=0.5 %
435000 psi
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 7.0
@Frequency 1e+6 Hz
7.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.24
@Frequency 1e+6 Hz
0.24
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 575 V575 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 °C428 °FDIN 53765
Maximum Service Temperature, Air 135 °C275 °Ffor 50% loss of tensile strength after 20000hr
 165 °C329 °Ffor 50% loss of tensile strength after 5000hr
 200 °C392 °F
Decomposition Temperature >= 310 °C>= 590 °F
Ignition Temperature >= 400 °C>= 752 °FASTM D129
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 260 °C500 °FFeed Zone
Zone 2 270 °C518 °FCompression
Zone 3 280 °C536 °FMetering-zone
Zone 4 280 °C536 °FNozzle
Melt Temperature 270 - 290 °C518 - 554 °FInjection-molding/Extrusion
 280 °C536 °FOptimal
Mold Temperature 80.0 °C176 °FOptimal
 80.0 - 90.0 °C176 - 194 °FInjection-molding
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Optimal
 <= 0.15 %<= 0.15 %
 
Descriptive Properties
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry)
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry)
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned)
Covestro Bayblend® FR3000 PC/ABS Blend

PBASG0263 / 131896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.