MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hybrid Plastics POSS® EP 2000 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: EP2000 is a POSS® based, ultra-high temperature epoxy adhesive. The POSS® content in EP2000 offers unique properties such as high thermal stability, outstanding oxygen and chemical resistance. It provides an exceptional transparent adhesive in these high temperature conditions for metallic, molded plastic and composite materials. Major applications include composites, medical devices, and electronics.

Information provided by Hybrid Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³after cure
Viscosity <= 5000 cP<= 5000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383
Modulus of Elasticity 1.00 - 1.50 GPa145 - 218 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C
@Temperature 20.0 °C
83.3 µin/in-°F
@Temperature 68.0 °F
Glass Transition Temp, Tg >= 300 °C>= 572 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 6.00 min
@Temperature 80.0 °C
0.100 hour
@Temperature 176 °F
Pot Life 180 min180 min
Shelf Life 6.00 - 12.0 Month6.00 - 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System
Master Bond LED401LV One Component, Moderate Viscosity LED Curable System
Master Bond EP46HT-2 Two Component, Heat Resistant Epoxy System
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating
Master Bond EP126 Two Component Toughened Epoxy Adhesive System

PHYBR031 / 78841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.