MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP46HT-2 Two Component, Heat Resistant Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, High Temperature

Material Notes: Key Features:
  • Glass transition temperature (Tg) of 220°C
  • Requires oven curing
  • Long working life
  • Superior adhesion to many substrates
  • Service temperature range from -100°F to 550°F
  • Withstands prolonged exposure to hostile environments
Product Description: Master Bond EP46HT-2 is a versatile two component epoxy system that can be used for bonding, sealing, coating and casting. It is most prominent for its temperature resistance along with the capability of withstanding aggressive chemicals. Its service temperature range extends from -100°F to +550°F. It is 100% reactive and does not contain any solvents or diluents. It is formulated to cure rapidly and requires a minimum curing temperature of 250°F; although a variety of cure schedules are possible. It should be noted that the mix ratio is a very forgiving 100 to 30-35 parts by weight. Upon curing, EP46HT-2 has a wide array of impressive physical and mechanical properties. It bonds well to a variety of substrates including metals, composites, ceramics, glass, rubbers and many plastics. One of the more noteworthy attributes of this system is its chemical resistance profile, which includes the ability to withstand many acids, bases, oils, fuels, hydrocarbons and solvents. It is also a very good electrical insulator. Unlike the EP46HT-1 product series, this line is not exothermic and can be used for potting and encapsulation. The color of Part A is clear; the color of Part B is brown. Master Bond EP46HT-2 is primarily used in specialty aerospace, electronic, petrochemical and OEM applications where high temperature resistance and the ability to withstand hostile chemicals is desirable.

Product Advantages:

  • Very forgiving mix ratio
  • Long open time at room temperature
  • Excellent temperature resistance and thermal stability
  • Capable of withstanding disruptive chemicals
  • High bonding strength to a wide variety of substrates
  • Top notch electrical insulation properties

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 50 - 350 cP50 - 350 cPPart B
 12000 - 20000 cP12000 - 20000 cPmixed
 60000 - 110000 cP60000 - 110000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
Tensile Strength >= 68.9 MPa>= 10000 psi
Tensile Modulus >= 2.76 GPa>= 400 ksi
Adhesive Bond Strength >= 17.2 MPa>= 2500 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cm
Dielectric Strength 17.7 kV/mm
@Thickness 3.17 mm
450 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 35.0 µm/m-°C16.7 - 19.4 µin/in-°F
Maximum Service Temperature, Air 288 °C550 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg 220 °C428 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 180 min2.00 - 3.00 hourPost cure for optimum properties at 350-400°F
 180 - 240 min
@Temperature 121 - 149 °C
3.00 - 4.00 hour
@Temperature 250 - 300 °F
Working Life >= 1440 min>= 1440 minAfter mixing, 100 g batch
Shelf Life 6.00 Month
@Temperature <=23.9 °C
6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Mixing Ratio100:30-35 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System
Master Bond EP113 Two Component Epoxy
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy
Master Bond EP121AO Thermally Conductive, Dimensionally Stable Epoxy System
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy

PMASTM886 / 185479

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.