MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow AFFINITY™ VP 8770 Polyolefin Plastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: AFFINITY® VP 8770 polyolefin plastomer is an alpha-olefin resin for general purpose applications. It exhibits excellent optics and flexibility. Its low specific gravity can help control resin and production costs, while reducing the weight of end products.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.885 g/cc0.0320 lb/in³
Melt Flow 1.0 g/10 min
@Load 2.16 kg
1.0 g/10 min
@Load 4.76 lb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Tensile Strength, Ultimate 22.1 MPa3210 psi
Tensile Strength, Yield 3.20 MPa464 psi
Elongation at Break >= 1000 %>= 1000 %
Tensile Modulus 0.0221 GPa3.21 ksi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ SE 1400 Polyolefin Plastomer
Dow AFFINITY™ SM 8400 Polyolefin Elastomer
Dow ATTANE™ 4201G, 2mil Ultra Low Density Ethylene/Octene Copolymer
Dow ATTANE™ 4401 Ultra Low Density Polyethylene, Blown Film Grade
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer

PDW412 / 34481

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.