System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Dow ATTANE™ 4201G, 2mil Ultra Low Density Ethylene/Octene Copolymer
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyethylene (PE)
;
Low Density (LDPE)
Material Notes:
ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.912
g/cc
0.0329
lb/in³
ASTM D792
Water Vapor Transmission
10.5
g/m²/day
@Pressure 0.101 MPa,
Temperature 38.0 °C
0.676
g/100 in²/day
@Pressure 14.7 psi,
Temperature 100 °F
100% RH; ASTM D1249
Oxygen Transmission
280
cc-mm/m²-24hr-atm
711
cc-mil/100 in²-24hr-atm
ASTM D3985
Carbon Dioxide Transmission
1235
cc-mm/m²-24hr-atm
3138
cc-mil/100 in²-24hr-atm
Dow Method
Thickness
50.8
microns
2.00
mil
Melt Flow
1.0
g/10 min
1.0
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Film Tensile Strength at Yield, MD
9.136
MPa
1325
psi
ASTM D882
Film Tensile Strength at Yield, TD
9.080
MPa
1317
psi
ASTM D882
Film Elongation at Break, MD
658 %
658 %
ASTM D882
Film Elongation at Break, TD
758 %
758 %
ASTM D882
Secant Modulus, MD
0.130
GPa
18.9
ksi
2% Secant; ASTM D882
Secant Modulus, TD
0.154
GPa
22.3
ksi
2% Secant; ASTM D882
Impact
260
260
[ft-lbf/in
3
]; Puncture Resistance; Dow Method
Elmendorf Tear Strength MD
1039
g
1039
g
ASTM D1922
Elmendorf Tear Strength TD
1232
g
1232
g
ASTM D1922
Elmendorf Tear Strength, MD
20.45
g/micron
519.5
g/mil
ASTM D1922
Elmendorf Tear Strength, TD
24.3
g/micron
616
g/mil
ASTM D1922
Dart Drop Test
607
g
1.34
lb
Method B; ASTM D1709
Film Tensile Strength at Break, MD
49.82
MPa
7226
psi
ASTM D882
Film Tensile Strength at Break, TD
45.84
MPa
6649
psi
ASTM D882
Heat Seal Strength Initiation Temperature
97.0
°C
207
°F
2 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Thermal Properties
Metric
English
Comments
Melting Point
123
°C
253
°F
Dow Method (DSC)
Vicat Softening Point
93.0
°C
199
°F
ASTM D1525
Optical Properties
Metric
English
Comments
Haze
8.0 %
8.0 %
ASTM D1003
Gloss
71 %
71 %
45°; ASTM D2457
Transmission, Visible
98 %
98 %
Clarity; ASTM D1746
Compliance Properties
Metric
English
Comments
FDA
Yes
Yes
See notes for details.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer
Dow AFFINITY™ VP 8770 Polyolefin Plastomer
Dow ATTANE™ 4401 Ultra Low Density Polyethylene, Blown Film Grade
Dow Engage® ENR 8556.00 Ethylene-Octene Copolymer
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
PDOW1194 / 30412
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.