Sarcon XR-e and XR-j are highly conformable/thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and make reliable and complete physical contact. GR-Hn has a hardened top surface Information provided by Fujipoly Industries |