MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.

Data Provided by the manufacturer, Coors Ceramics Co.

Key Words: Al2O3; aluminum oxide, alumina
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.80 g/cc0.137 lb/in³ASTM C20
Water Absorption 0.00 %0.00 %ASTM C373
Particle Size 6.0 µm6.0 µmAverage Crystal Size - Thin Section Test
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 13.713.71000 g load
Hardness, Rockwell 45 N 8282GPa
Tensile Strength, Ultimate 248 MPa36000 psiACMA Test #4
Modulus of Elasticity 350 GPa50800 ksiASTM C848
Flexural Strength 375 MPa54400 psiASTM F417
Compressive Strength 2500 MPa363000 psiASTM C773
Poissons Ratio 0.220.22ASTM C848
Fracture Toughness 4.00 - 5.00 MPa-m½3.64 - 4.55 ksi-in½
Shear Modulus 143 GPa20700 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D1829
 2.00e+6 ohm-cm
@Temperature 1000 °C
2.00e+6 ohm-cm
@Temperature 1830 °F
ASTM D1829
 2.00e+10 ohm-cm
@Temperature 500 °C
2.00e+10 ohm-cm
@Temperature 932 °F
ASTM D1829
Dielectric Constant 9.6
@Frequency 1e+6 Hz
9.6
@Frequency 1e+6 Hz
Dielectric Strength 8.70 kV/mm221 kV/inac; ASTM D116
Dielectric Loss Index 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
ASTM D2520
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.20 µm/m-°C
@Temperature 25.0 - 1000 °C
4.56 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C372
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°FASTM E1269
Thermal Conductivity 27.5 W/m-K191 BTU-in/hr-ft²-°FASTM C408
Maximum Service Temperature, Air 1700 °C3090 °FNo Load
 
Component Elements PropertiesMetricEnglishComments
Al2O3 98.5 %98.5 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec B 601 Alumina, 98.5%
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3)
CeramTec 771 94% Alumina (Al2O3)
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2
CeramTec AT 79 Alumina, 99.6%

CA7E / 380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.