MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyPLASTY PolyJARID PA 6 E Polyamide 6 extruded, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes:
  • Extrusion: Extruded profiles according to drawings and semi-products according to DIN
  • Machine parts: Turned and milled parts in single and serial production

Information provided by PolyPLASTY.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption 3.0 %3.0 %under regular conditions; ISO 62
Moisture Absorption at Equilibrium 9.5 %9.5 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, H358/30 150 MPa21800 psiISO 2039-1
Hardness, Shore D 8282ISO 868, ISO 2039-2
Tensile Strength, Yield 80.0 MPa11600 psiISO 527
Elongation at Break 70 %70 %ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
Modulus of Elasticity 3.00 GPa435 ksiISO 527
Flexural Strength 125 MPa18100 psiISO 178
Fatigue Strength 33.0 MPa4790 psiflexure; ASTM D671
Izod Impact, Notched (ISO) 8.30 kJ/m²3.95 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1C
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1C
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179/1eA
Tensile Creep Modulus, 1000 hours 2900 MPa421000 psi0.5 percent; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 50 Hz
4.0
@Frequency 50 Hz
IEC 60250
Dielectric Strength 100 kV/mm
@Thickness 0.600 mm
2540 kV/in
@Thickness 0.0236 in
IEC 60243-1
Dissipation Factor  0.010
@Frequency 50 Hz
0.010
@Frequency 50 Hz
IEC 60250
 0.30
@Frequency 1e+6 Hz
0.30
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 70.0 µm/m-°C38.9 µin/in-°FISO 11359
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°FIEC 1006
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FDIN 52 612
Maximum Service Temperature, Air 90.0 °C194 °Flong term
 180 °C356 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C149 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75
Vicat Softening Point 204 °C
@Load 5.10 kg
399 °F
@Load 11.2 lb
point B; ISO 306 VST/B/50
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 
Descriptive Properties
LOI Acid Index (%)25ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nylacast PA6C Cast Nylon 6
PolyPLASTY PolyPOM Polyoxymethylene (POM)

PPOLYPL921 / 197631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.