MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyPLASTY PolyPOM Polyoxymethylene (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: POM has minimal water absorption, excellent dimensional stability and the best properties for chip machining. Thanks to its favorable characteristics, great hardness, rigidity and strength with good toughness, chemical resistance and its shear behavior with abrasion resistance, POM is a successful replacement for metal materials. It is resistant to organic solvents. It also features good resistance to black light UV-radiation.

Information provided by PolyPLASTY.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.20 %0.20 %under regular conditions; ISO 62
Moisture Absorption at Equilibrium 0.80 %0.80 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, H358/30 145 MPa21000 psiISO 2039-1
Hardness, Shore D 8181ISO 868, ISO 2039-2
Elongation at Break 27 %27 %ISO 527
Elongation at Yield 9.4 %9.4 %ISO 527
Modulus of Elasticity 2.70 GPa392 ksiISO 527
Flexural Strength 97.0 MPa14100 psiISO 178
Fatigue Strength 31.0 MPa4500 psiflexure; ASTM D671
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inISO 180/4A
Izod Impact, Notched (ISO)  5.50 kJ/m²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 5.50 kJ/m²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  100 kJ/m²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1C
 930 kJ/m²
@Temperature 23.0 °C
443 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1C
Charpy Impact Unnotched  19.0 J/cm²
@Temperature -30.0 °C
90.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 21.0 J/cm²
@Temperature 23.0 °C
99.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 1400 MPa203000 psi0.5 percent; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  3.8
@Frequency 50 Hz
3.8
@Frequency 50 Hz
IEC 60250
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm
@Thickness 1.00 mm
1020 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0010
@Frequency 50 Hz
0.0010
@Frequency 50 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359
Specific Heat Capacity 1.47 J/g-°C0.351 BTU/lb-°FIEC 1006
Thermal Conductivity 0.310 W/m-K2.15 BTU-in/hr-ft²-°FDIN 52 612
Maximum Service Temperature, Air 90.5 °C195 °Flong term
 140 °C284 °Fshort term
Vicat Softening Point 150 °C
@Load 5.10 kg
302 °F
@Load 11.2 lb
point B; ISO 306 VST/B/50
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 
Descriptive Properties
LOI Acid Index (%)15ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
VICTREX™ PEEK 450G™ General Purpose
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
DuPont Mobility and Materials Zytel® EFE1068 NC010T PA66
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced

PPOLYPL928 / 197638

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.