MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 7C27Mo2 flapper valve steel Strip
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel

Material Notes: Sandvik 7C27Mo2 is a hardened and tempered martensitic stainless steel alloyed with molybdenum. The material is characterized by:
  • High strength
  • Very high fatigue strength under bending and impact stress
  • Excellent surface finish
  • High compressive residual surface stress
  • Low levels of non-metallic inclusions
  • Good wear resistance
Sandvik 7C27Mo2 flapper valve steel has good dimensional tolerances and good flatness.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1800 MPa261000 psi
Tensile Strength, Yield  1300 MPa
@Strain 0.05 %
189000 psi
@Strain 0.05 %
 1450 MPa
@Strain 0.2 %
210000 psi
@Strain 0.2 %
Elongation at Break >= 5.0 %>= 5.0 %
Modulus of Elasticity 210 GPa30500 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.5 µm/m-°C
@Temperature 30.0 - 100 °C
5.83 µin/in-°F
@Temperature 86.0 - 212 °F
 11.0 µm/m-°C
@Temperature 30.0 - 200 °C
6.11 µin/in-°F
@Temperature 86.0 - 392 °F
 11.5 µm/m-°C
@Temperature 30.0 - 300 °C
6.39 µin/in-°F
@Temperature 86.0 - 572 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 50.0 - 100 °C
0.110 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 24.0 W/m-K167 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 %0.38 %
Chromium, Cr 13.5 %13.5 %
Manganese, Mn 0.55 %0.55 %
Molybdenum, Mo 1.0 %1.0 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si 0.40 %0.40 %
Sulfur, S <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik 7C27Mo2 Strip Steel
Sandvik Bioline 7C27Mo2 Strip steel
Sandvik Chromflex 7C27Mo2 Strip steel
Bohler-Uddeholm moldMAX® XL High Strength Copper Alloy
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel

NSANDV5170 / 199734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.