MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically engineered for cavities, cores and inserts, and a broad range of product applications that demand superior surface finish. Examples include optical, ultra clean medical applications and CD/DVD applications.

POLMAX® is characterized by:

  • Excellent polishability
  • Good corrosion resistance
  • Good wear resistance
  • Good machinability
  • Good stability in hardening

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.81 g/cc0.282 lb/in³hardened to 52 HRC
 7.67 g/cc
@Temperature 399 °C
0.277 lb/in³
@Temperature 750 °F
hardened to 52 HRC
 7.75 g/cc
@Temperature 199 °C
0.280 lb/in³
@Temperature 390 °F
hardened to 52 HRC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200200Soft annealed (Delivery condition)
Hardness, Rockwell C 30 - 5830 - 58tempering temp 200 - 1200°F
Tensile Strength, Ultimate 2070 MPa300000 psihardened to 52 HRC
Tensile Strength, Yield 1610 MPa
@Strain 0.2 %
234000 psi
@Strain 0.2 %
hardened to 52 HRC
Modulus of Elasticity 200 GPa29000 ksi(hardened to 52 HRC)
 180 GPa
@Temperature 399 °C
26100 ksi
@Temperature 750 °F
hardened to 52 HRC
 190 GPa
@Temperature 199 °C
27600 ksi
@Temperature 390 °F
hardened to 52 HRC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 199 °C
6.10 µin/in-°F
@Temperature 390 °F
hardened to 52 HRC
 11.5 µm/m-°C
@Temperature 399 °C
6.40 µin/in-°F
@Temperature 750 °F
hardened to 52 HRC
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
hardened to 52 HRC
Thermal Conductivity  16.0 W/m-K
@Temperature 20.0 °C
111 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
hardened to 52 HRC
 20.0 W/m-K
@Temperature 199 °C
139 BTU-in/hr-ft²-°F
@Temperature 390 °F
hardened to 52 HRC
 24.0 W/m-K
@Temperature 399 °C
167 BTU-in/hr-ft²-°F
@Temperature 750 °F
hardened to 52 HRC
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 %0.38 %
Chromium, Cr 13.6 %13.6 %
Iron, Fe 84.3 %84.3 %as balance
Manganese, Mn 0.50 %0.50 %
Silicon, Si 0.90 %0.90 %
Vanadium, V 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM RAMAX® LH Plastic Mold Steel
420 Stainless Steel
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420

NBUCOR25 / 15494

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.