MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 390.0-T5 Conventional Die Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: AA390.0-T5; UNS A03900; Aluminium 390.0-T5; Al390.0-T5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.72 g/cc0.0983 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 125125500 kg load, 10 mm ball
Hardness, Knoop 157157Estimated from Brinell Hardness.
Hardness, Rockwell A 4848Estimated from Brinell Hardness.
Hardness, Rockwell B 7777Estimated from Brinell Hardness.
Hardness, Vickers 143143Estimated from Brinell Hardness.
Tensile Strength, Ultimate 295 MPa42800 psi
Tensile Strength, Yield 260 MPa
@Strain 0.2 %
37700 psi
@Strain 0.2 %
Elongation at Break 1.0 %1.0 %in 50 mm
Tensile Modulus 81.2 GPa11800 ksi
Compressive Modulus 82.8 GPa12000 ksi
Machinability 10 %10 %0-100 Scale (100=best)
Shear Strength 178 MPa25800 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000680 ohm-cm0.00000680 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  18.0 µm/m-°C
@Temperature 20.0 - 100 °C
10.0 µin/in-°F
@Temperature 68.0 - 212 °F
 22.5 µm/m-°C
@Temperature 20.0 - 300 °C
12.5 µin/in-°F
@Temperature 68.0 - 572 °F
Estimated by MatWeb from similar alloys
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°FTypical for cast aluminum
Thermal Conductivity 134 W/m-K930 BTU-in/hr-ft²-°F
Melting Point 507 - 649 °C945 - 1200 °F
Solidus 507 °C945 °F
Liquidus 649 °C1200 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 496 °C925 °F
Aging Temperature 232 °C450 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 74.4 - 79.6 %74.4 - 79.6 %As remainder
Copper, Cu 4.0 - 5.0 %4.0 - 5.0 %
Iron, Fe <= 1.3 %<= 1.3 %
Magnesium, Mg 0.45 - 0.65 %0.45 - 0.65 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.20 %<= 0.20 %
Silicon, Si 16 - 18 %16 - 18 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 518.0-F Die Casting Alloy
Aluminum LM4 TF (T6) Temper, Gravity Die Cast
Aluminum B390.0-F Die Casting Alloy
Aluminum 390.0-F Conventional Die Cast
Aluminum A360.0-F Die Casting Alloy

MAC3900T5C / 10063

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.