MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay FM® 73 Epoxy Film Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 73 film adhesive is a toughened, general purpose aerospace epoxy designed to provide excellent structural performance from -67°F to 180°F (-55°C to 82°C). FM 73 film adhesive is formulated to provide outstanding durability in bonding metals and is also suitable for boding many structural composite systems. Extensive testing has proven that FM 73 adhesive meets stringent environmental resistance and bonding durability requirements. To achieve maximum environmental resistance and bonding durability the use of BR® 127 corrosion inhibiting primer is recommended in bonding metallic components.

Features & Benefits:

  • Demonstrates excellent peel strength and structural performance from -67°F to 180°F (-55°C to 82°C)
  • Resistant to pre-bond humidity exposure
  • Good moisture and corrosion resistance in high humidity
  • Shop life of 15 days at 75°F (24°C)
Applications:
  • Metal-to-metal bonding
  • Composite-to-composite bonding
  • Composite-to-metal bonding

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.25 %<= 1.25 %
Outgassing - Total Mass Loss 0.78 %0.78 %TWL
Collected Volatile Condensable Material 0.00 %0.00 %
Storage Temperature <= -18.0 °C<= -0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  4.55 MPa
@Temperature 82.0 °C
660 psi
@Temperature 180 °F
Flatwise, 0.06 lb/ft2
 6.07 MPa
@Temperature 82.0 °C
880 psi
@Temperature 180 °F
Flatwise, 0.085 lb/ft2
 8.96 MPa
@Temperature 24.0 °C
1300 psi
@Temperature 75.2 °F
Flatwise, 0.06 lb/ft2
 9.65 MPa
@Temperature 24.0 °C
1400 psi
@Temperature 75.2 °F
Flatwise, 0.085 lb/ft2
 11.6 MPa
@Temperature -55.0 °C
1680 psi
@Temperature -67.0 °F
Flatwise, 0.06 lb/ft2
 11.9 MPa
@Temperature -55.0 °C
1730 psi
@Temperature -67.0 °F
Flatwise, 0.085 lb/ft2
Shear Strength 35.4 MPa5140 psi0.06 lb/ft2, 30 days at 120°F (50°C) and 95 – 100% R.H.
 35.4 MPa5140 psi0.06 lb/ft2, 7 days immersion in hydrocarbon fluid (TT-S-735)
 36.1 MPa5230 psi0.06 lb/ft2, 7 days immersion in JP-4 fuel (MIL-J-5624)
 36.1 MPa5240 psi0.06 lb/ft2, 30 days salt spray
 36.3 MPa5270 psi0.06 lb/ft2, 30 days salt spray
 28.1 MPa
@Temperature 82.0 °C
4080 psi
@Temperature 180 °F
Blister, Metal-to-Metal, 0.06 lb/ft2
 28.4 MPa
@Temperature 82.0 °C
4120 psi
@Temperature 180 °F
Blister, Metal-to-Metal, 0.085 lb/ft2
 29.9 MPa
@Temperature 82.0 °C
4340 psi
@Temperature 180 °F
Metal-to-Metal, 0.06 lb/ft2
 32.9 MPa
@Temperature 82.0 °C
4770 psi
@Temperature 180 °F
Metal-to-Metal, 0.085 lb/ft2
 34.8 MPa
@Temperature 24.0 °C
5050 psi
@Temperature 75.2 °F
Blister, Metal-to-Metal, 0.085 lb/ft2
 35.2 MPa
@Temperature 24.0 °C
5100 psi
@Temperature 75.2 °F
Blister, Metal-to-Metal, 0.06 lb/ft2
 36.5 MPa
@Temperature -55.0 °C
5290 psi
@Temperature -67.0 °F
Blister, Metal-to-Metal, 0.085 lb/ft2
 37.6 MPa
@Temperature -55.0 °C
5460 psi
@Temperature -67.0 °F
Blister, Metal-to-Metal, 0.06 lb/ft2
 44.8 MPa
@Temperature 24.0 °C
6500 psi
@Temperature 75.2 °F
Metal-to-Metal, 0.06 lb/ft2
 45.9 MPa
@Temperature -55.0 °C
6650 psi
@Temperature -67.0 °F
Metal-to-Metal, 0.06 lb/ft2
 46.2 MPa
@Temperature -55.0 °C
6700 psi
@Temperature -67.0 °F
Metal-to-Metal, 0.085 lb/ft2
 47.2 MPa
@Temperature 24.0 °C
6840 psi
@Temperature 75.2 °F
Metal-to-Metal, 0.085 lb/ft2
Peel Strength  9.12 kN/m
@Temperature -55.0 °C
52.0 pli
@Temperature -67.0 °F
Floating Roller metal-to-metal, 0.085 lb/ft2; ASTM D3167-76
 11.4 kN/m
@Temperature 24.0 °C
65.0 pli
@Temperature 75.2 °F
Floating Roller metal-to-metal, 0.06 lb/ft2; ASTM D3167-76
 11.6 kN/m
@Temperature -55.0 °C
66.0 pli
@Temperature -67.0 °F
Floating Roller metal-to-metal, 0.06 lb/ft2; ASTM D3167-76
 13.8 kN/m
@Temperature 24.0 °C
79.0 pli
@Temperature 75.2 °F
Floating Roller metal-to-metal, 0.085 lb/ft2; ASTM D3167-76
 16.8 kN/m
@Temperature 82.0 °C
96.0 pli
@Temperature 180 °F
Floating Roller metal-to-metal, 0.06 lb/ft2; ASTM D3167-76
 19.3 kN/m
@Temperature 82.0 °C
110 pli
@Temperature 180 °F
Floating Roller metal-to-metal, 0.085 lb/ft2; ASTM D3167-76
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.0 °C180 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorYellow0.18 mm
 Yellow0.25 mm
 Yellow0.38 mm
Metal-to-Metal Climbing Drum Peel330 Nm/m-55°C, 0.06 lb/ft2, ASTM D1781-76
 390 Nm/m-55°C, 0.085 lb/ft2, ASTM D1781-76
 420 Nm/m24°C, 0.06 lb/ft2, ASTM D1781-76
 56 Nm/m82°C, 0.06 lb/ft2, ASTM D1781-76
 650 Nm/m24°C, 0.085 lb/ft2, ASTM D1781-76
 690 Nm/m82°C, 0.085 lb/ft2, ASTM D1781-76
Sandwich Peel130 Nm/m-55°C, 0.085 lb/ft2
 140 Nm/m24°C, 0.06 lb/ft2
 220 Nm/m24°C, 0.085 lb/ft2
 61 Nm/m82°C, 0.06 lb/ft2
 79 Nm/m-55°C, 0.06 lb/ft2
 96 Nm/m82°C, 0.085 lb/ft2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay FM® 73M Epoxy Film Adhesive
Solvay FM® 300M Epoxy Film Adhesive
Henkel Hysol EA 9313 Paste Adhesive System
Solvay FM® 300 Epoxy Film Adhesive
Henkel Hysol EA 9330 Paste Adhesive System

PCYTED046 / 180348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.