MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total SB 1359 High Density Polyethylene - Injection Stretch Blow Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: HDPE SB 1359 is a high density polyethylene with outstanding compromise between stiffness and Environmental Stress Crack Resistance. It has been specifically designed for the manufacture of packaging for household, industrial and cosmetics liquids. HDPE SB 1359 is also suitable for food applications.

Its unique molecular design allows it to be used in Injection Stretch Blow Molding process (ISBM). It combines an easy processing both during the injection of preforms and during the reheating and stretching phase on the blowing machines.

HDPE SB 1359 is a pellet grade and contains antioxidants.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.959 g/cc0.959 g/ccISO 1183
Environmental Stress Crack Resistance >= 100 hour>= 100 hourF50, Anatarox 100%; ASTM D 1693B
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 1.30 GPa189 ksiISO 178
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 240 °C428 - 464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total SB 1461 High Density Polyethylene - Injection Stretch Blow Molding
LyondellBasell Alathon® H5656 High Density Polyethylene, Injection Molding Grade
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
LyondellBasell Purell PE3020D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding

PTOTAL729 / 130454

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.