MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® H5656 High Density Polyethylene, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: ALATHON H5656 is a high-flow injection molding grade of resin designed for thin-wall molding. This resin exhibits enhanced processing and thermal stability for fast cycling in multi-cavity stack molds, good color and organoleptic properties. Typical applications include rigid packaging such as promotional drink cups and deli containers.

Regulatory Status: H5656 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.593 - 0.625 g/cc0.0214 - 0.0226 lb/in³ASTM D1895
Density 0.956 g/cc0.0345 lb/in³ASTM D1505
Melt Flow 56 g/10 min
@Load 2.16 kg,
Temperature 190 °C
56 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 51.3 cm20.2 inEquistar test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7171ASTM D2240
Tensile Strength at Break 28.8 MPa4180 psi50 mm/min; ASTM D638
Elongation at Break 3.2 %3.2 %50 mm/min; ASTM D638
Tensile Modulus 0.717 GPa104 ksi1% Secant; 50mm/min; ASTM D638
 0.862 GPa125 ksi50mm/min; ASTM D638
Flexural Modulus 1.07 GPa155 ksi2% Secant; 12.5 mm/min; ASTM D790
 1.39 GPa201 ksi12.5 mm/min; ASTM D790
Flexural Modulus, 1% Secant 1280 MPa186000 psi1% Secant; 12.5 mm/min; ASTM D790
Izod Impact, Notched 0.203 J/cm0.380 ft-lb/inASTM D256
 2.56 J/cm
@Temperature -18.0 °C
4.80 ft-lb/in
@Temperature -0.400 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Melting Point 129.3 °C264.7 °FASTM D3418
Crystallization Temperature 114.8 °C238.6 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C165 °FASTM D648
Vicat Softening Point 123 °C253 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 °C450 °F
Middle Barrel Temperature 243 °C470 °F
Front Barrel Temperature 246 °C475 °F
Nozzle Temperature 246 °C475 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding
Ineos J50-1000-178 HDPE
LyondellBasell Alathon M 6020SB High Denisty Polyethylene

PEQU0787 / 104143

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.