MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos Nova S-5400 High Impact Compact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Impact polystyrene with high dimensional stability under heat, particularly suitable fore extrusion and thermoforming of technical parts or packaging applications but also used for injection molding applications where a high stiffness and impact strength are required. For injection molding generally a lubricated type is used.

All mechanical properties measured under standard conditions 50% RH and 23°C.

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³DIN 53479
Water Absorption <= 0.10 %<= 0.10 %DIN 53495
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
DIN 5375/ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 110 MPa16000 psiDIN 53456
Tensile Strength, Ultimate 40.0 MPa5800 psiDIN 53455
Elongation at Break 20 %20 %DIN 53455
Modulus of Elasticity 2.30 GPa334 ksiDIN 53457
Flexural Yield Strength 65.0 MPa9430 psiDIN 53452
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²Low Temp; DIN 53453
 7.00 kJ/m²3.33 ft-lb/in²DIN 53453/ISO 179
Izod Impact, Unnotched (ISO) 70.0 kJ/m²33.3 ft-lb/in²DIN 53453
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°FDIN 52612
Vicat Softening Point 94.0 °C201 °FDIN 53460

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lacqrene® 4241 High Impact Polystyrene
Total PSC 523 Polystyrene
Total PSI 4440(AS) High Impact Polystyrene
Total Lacqrene® 1235 High Impact Polystyrene
RTP Company RTP 400 Polystyrene (PS), General Purpose

PNOVA094 / 54995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.