MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Lacqrene® 1235 High Impact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: LACQRENE® 1235 is a high gloss, high impact polystyrene used in injection molding and co-extrusion. This grade produces articles with a surface gloss level equivalent to that of certain grades of ABS.

Applications: Toys, Office equipment, White goods, Telephones, Video cassette shutters, Glossy items by coextrusion. Translucent products by blending with 1240.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption <= 0.10 %<= 0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in
Melt Flow 5.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
5.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7575ISO 2039-2
Tensile Strength at Break 25.0 MPa3630 psiISO 527-2
Tensile Strength, Yield 31.0 MPa4500 psiISO 527-2
Elongation at Break 30 %30 %ISO 527-2
Tensile Modulus 2.05 GPa297 ksiISO 527-2
Flexural Modulus 2.05 GPa297 ksiISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmISO IEC93
Dielectric Strength 150 kV/mm3810 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 91.0 µm/m-°C
@Temperature 20.0 °C
50.6 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FAnnealed; ISO 75-2B
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C163 °FUnannealed; ISO 75-2A
Vicat Softening Point 89.0 °C192 °F50N (T° increase = 5°C/h); ISO 306B50
 97.0 °C207 °F10N (T° increase = 50°C/h); ISO 306A50

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lacqrene® 4241 High Impact Polystyrene
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
Aclo Accucomp Polystyrene HS0600L High Impact
Americas Styrenics Styron® 425 High Impact Polystyrene
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin

PFINAA022 / 38458

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.