MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CRP Technology Windform® GT Polyamide Glass Composite
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter. Windform® GT differs from the other Windform® powders thanks to its higher flexibility. Windform® GT combines optimal characteristics of elasticity and ductility and resistance, thus it can be considered a highly valuable material in various racing and functional applications affected to vibration and shocks. In fact, the material has meaningful values of impact strength and elongation at break, which combined with relevant values of tensile strength and flexural strength make it ideal for applications where resistance to “damage” is a prerequisite. Windform® is resistant to moisture. Windform® GT is also a very light weight material with excellent mechanical properties per unit density.

Applied in automotive applications where a certain flexibility in the car and under hood (such as snap fit) is required. It is also suitable in motorsport, air ducts, intake and cooling systems, the hydraulic ducts in contact with liquids or oils, in protective cover for sensors and for all applications that need a good flexibility and resistance to damage (for example: racing components near the ground).

Information provided by CRP Technology.

Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 56.21 MPa8153 psiUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Elongation at Break 14.82 %14.82 %UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Tensile Modulus 3.29 GPa477 ksiUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Flexural Strength 87.9 MPa12700 psiUNI EN ISO 14125: 2000
Flexural Modulus 3.227 GPa468.0 ksiUNI EN ISO 14125: 2000
Charpy Impact Unnotched 5.428 J/cm²25.83 ft-lb/in²ISO 179-1:2007
Charpy Impact, Notched 0.869 J/cm²4.14 ft-lb/in²ISO 179-1:2007
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.62e+15 ohm-cm2.62e+15 ohm-cmASTM D257-93
Surface Resistance 1.02e+16 ohm1.02e+16 ohmASTM D257-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 193 °C379 °FISO 11357-2
Deflection Temperature at 1.8 MPa (264 psi) 169.4 °C336.9 °FASTM D648
Vicat Softening Point 188.9 °C372.0 °F10 N; ASTM D1252
 
Descriptive Properties
ColorBlack
Specific Flexural Modulus2711.76[MPa/(g/cc)], Flexural Modulus per density unit
Specific Flexural Strength73.87[MPa/(g/cc)], Flexural Strength per density unit
Specific Tensile Modulus2764.54[MPa/(g/cc)], Tensile Modulus per density unit
Specific Tensile Strength47.24[MPa/(g/cc)], UTS per density unit
Surface Finish1.15 Ra µmAfter CNC Machining
 1.15 Ra µmAfter CNC machining
 6.2 Ra µmAfter SLS Process

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CRP Technology Windform® PS Polystyrene for Selective Laser Sintering
CRP Technology Windform® LX 2.0 Polyamide Composite
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage

PCRPT01 / 130415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.