MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAKEEP® Film 0FH90 PEEK  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: VESTAKEEP® film 0FH90 is a cast film based on 100% unreinforced polyether ether ketone (PEEK). The film is amorphous with a matte/glossy surface finish. The material features low extrusion related internal stresses and is ideal to thermoform 3D parts from, e.g. small speaker membranes.

Application examples:

  • electrical insulation
  • thermoformed thin parts
  • loudspeaker membranes
Important notice: Amorphous PEEK film undergoes crystallization at above its glass transition temperature around 150°C. This should be taken into account upon processing as well as in final applications. The crystallization can only be reversed by heating to the melt followed by quenching.

VESTAKEEP® film properties include:

  • High continuous use temperature
  • Excellent chemical resistance
  • Tough and impact resistant
  • Low creep
  • Low abrasion, low coefficient of friction
  • Low water absorption
  • Electrical insulation
  • Low flammability
  • Free of flame retardants, no halogens
  • Approved for food contact
  • Low weight
  • Recyclable (neat PEEK resin)
  • Stabile towards ionizing irradiation
  • RoHS compliant
Secondary processes: VESTAKEEP films can be processed by many secondary processes, e.g.:
  • Die and water-jet cutting
  • Surface treatment (corona, plasma, flame)
  • Thermoforming
  • Adhesive bonding
  • Welding, sealing, printing

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc
@Thickness 0.0250 mm
0.0455 lb/in³
@Thickness 0.000984 in
ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa
@Thickness 0.0250 mm
13100 psi
@Thickness 0.000984 in
100 mm/min; ISO 527-3
Tensile Strength, Yield 60.0 MPa
@Thickness 0.0250 mm
8700 psi
@Thickness 0.000984 in
100 mm/min; ISO 527-3
Elongation at Break >= 150 %
@Thickness 0.0250 mm
>= 150 %
@Thickness 0.000984 in
100 mm/min; ISO 527-3
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
 1.00e+15 ohm1.00e+15 ohmSpec.; IEC 60093
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 2.8
@Frequency 50 Hz
2.8
@Frequency 50 Hz
IEC 60250
 2.9
@Frequency 1000 Hz
2.9
@Frequency 1000 Hz
IEC 60250
Dielectric Strength  140 kV/mm
@Thickness 0.125 mm
3560 kV/in
@Thickness 0.00492 in
amorphous; IEC 60243-1
 190 kV/mm
@Thickness 0.0750 mm
4830 kV/in
@Thickness 0.00295 in
amorphous; IEC 60243-1
Dielectric Breakdown  13500 V
@Thickness 0.0750 mm
13500 V
@Thickness 0.00295 in
amorphous; IEC 60243-1
 17500 V
@Thickness 0.125 mm
17500 V
@Thickness 0.00492 in
amorphous; IEC 60243-1
Dissipation Factor  0.0030
@Frequency 1000 Hz
0.0030
@Frequency 1000 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V175 V100 drops value; IEC 60112
 200 V200 VCTI; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature >= 165 °C
@Thickness 0.0250 mm
>= 329 °F
@Thickness 0.000984 in
Cold onset
Glass Transition Temp, Tg 150 °C
@Thickness 0.0250 mm
302 °F
@Thickness 0.000984 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Victrex APTIV™ 1300-050G Black Polyetheretherketone (PEEK) Polymer Film
Evonik VESTAKEEP® Film 0FH81 PEEK
Evonik VESTAKEEP® Film 0FH80 PEEK
Victrex APTIV™ 2000-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous
Covestro MAKROFOL® UV 503 9-2 060004 Polycarbonate Film

PEVONIL203 / 196407

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.