MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TechnylStar™ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This product is ideally suited for applications such as MCBs and contactors as well as being able to be used in many varied thin wall applications where its high flow polymer base enables it to achieve a UL94 V-0 rating down to a 0.4mm wall thickness. This product is available in a number of different colors including the standard Natural, light and dark Grey and Black. Specific colors and laser marking grades optimized for YAG and UV laser types are also available upon request.

For all products containing Flame additives Rhodia recomends the use of high Chromium, low Carbon coating for the steels (example CR19% C1.9%). The use of this steel can help to prevent corrosion, extend the equipment lifetime and allow greater parameter flexibility.

Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183-A
Water Absorption 0.90 %
@Time 86400 sec
0.90 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inRhodia EP test
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inRhodia EP test
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 97.0 MPa14100 psiConditioned; ISO 527 Type 1 A
 147 MPa21300 psiDAM; ISO 527 Type 1 A
Elongation at Break 2.28 %2.28 %DAM; ISO 527 Type 1 A
 5.27 %5.27 %Conditioned; ISO 527 Type 1 A
Tensile Modulus 7.01 GPa1020 ksiConditioned; ISO 527 Type 1 A
 11.76 GPa1706 ksiDAM; ISO 527 Type 1 A
Flexural Strength 169 MPa24500 psiConditioned; ISO 178
 243 MPa35200 psiDAM; ISO 178
Flexural Modulus 6.90 GPa1000 ksiConditioned; ISO 178
 10.68 GPa1549 ksiDAM; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²DAM; ISO 180/A
 12.0 kJ/m²5.71 ft-lb/in²Conditioned; ISO 180/A
Izod Impact, Unnotched (ISO) 54.0 kJ/m²25.7 ft-lb/in²DAM; ISO 180/1U
 63.0 kJ/m²30.0 ft-lb/in²Conditioned; ISO 180/1U
Charpy Impact Unnotched 6.70 J/cm²31.9 ft-lb/in²DAM; ISO 179/1eU
 6.90 J/cm²32.8 ft-lb/in²Conditioned; ISO 179/1eU
Charpy Impact, Notched 0.960 J/cm²4.57 ft-lb/in²DAM; ISO 179/1eA
 1.30 J/cm²6.19 ft-lb/in²Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.10e+14 ohm1.10e+14 ohmDAM; IEC 60093
Dielectric Constant 2.92.9DAM; IEC 60250
 4.354.35Conditioned; IEC 60250
Dielectric Strength 28.5 kV/mm724 kV/inConditioned; IEC 60243
 39.8 kV/mm1010 kV/inDAM; IEC 60243
Dissipation Factor 0.0800.080Conditioned; IEC 60250
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75/Af
Flammability, UL94  V-0
@Thickness 0.381 mm
V-0
@Thickness 0.0150 in
DAM; ISO 1210/UL94
 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
DAM; ISO 1210/UL94
Oxygen Index 35 %35 %DAM; ISO 4589
Glow Wire Ignition Temperature  775 °C
@Thickness 20.3 mm
1430 °F
@Thickness 0.800 in
Glow Wire Ignition Temp; DAM; IEC 60695-2-13
 800 °C
@Thickness 40.6 mm
1470 °F
@Thickness 1.60 in
Glow Wire Ignition Temp; DAM; IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 20.3 mm
1760 °F
@Thickness 0.800 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 40.6 mm
1760 °F
@Thickness 1.60 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 81.3 mm
1760 °F
@Thickness 3.20 in
DAM; IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 220 - 225 °C428 - 437 °F
Middle Barrel Temperature 225 - 235 °C437 - 455 °F
Front Barrel Temperature 235 - 245 °C455 - 473 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.15 %<= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry)

PRHO32 / 123362

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.