MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PSI 3351 High Heat Resistance Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Total Petrochemicals Polystyrene 3351 is a high heat resistance, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stability.

Suitable applications for Total Petrochemicals Polystyrene 3351 include TV Covers, printers, scanners and electrical appliances.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Water Absorption 0.070 %0.070 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 5.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
5.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Spiral Flow 46.0 cm
@Temperature 220 °C
18.1 in
@Temperature 428 °F
ASTM D3123
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9999ASTM D785
Tensile Strength at Break 30.0 MPa4350 psiASTM D638
Tensile Strength, Yield 32.0 MPa4640 psiASTM D638
Elongation at Break 55 %55 %ASTM D638
Tensile Modulus 2.20 GPa319 ksiASTM D638
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched (ISO) 9.50 kJ/m²4.52 ft-lb/in²ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmISO IEC 93
Dielectric Strength 150 kV/mm3810 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 91.0 µm/m-°C50.6 µin/in-°FASTM D696
Hot Ball Pressure Test 90.0 °C194 °FJET, 2.0 mm
Vicat Softening Point 100 °C
@Load 1.02 kg
212 °F
@Load 2.25 lb
50°C per hour; ASTM D1525
Heat Distortion Temperature 88.9 °C192 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lacqrene® 3351(AS) Impact Polystyrene
Overview of materials for Polystyrene, Heat Resistant Grade
Total PSI 4440(AS) High Impact Polystyrene

PTOTAL888 / 130613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.