MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PSI 3351 High Heat Resistance Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Total Petrochemicals Polystyrene 3351 is a high heat resistance, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stability.

Suitable applications for Total Petrochemicals Polystyrene 3351 include TV Covers, printers, scanners and electrical appliances.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Water Absorption 0.070 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 5.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
Spiral Flow 46.0 cm
@Temperature 220 °C
ASTM D3123
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 99ASTM D785
Tensile Strength at Break 30.0 MPaASTM D638
Tensile Strength, Yield 32.0 MPaASTM D638
Elongation at Break 55 %ASTM D638
Tensile Modulus 2200 MPaASTM D638
Flexural Modulus 2000 MPaASTM D790
Izod Impact, Notched (ISO) 9.50 kJ/m²ASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+13 ohmISO IEC 93
Dielectric Strength 150 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 91.0 µm/m-°CASTM D696
Hot Ball Pressure Test 90.0 °CJET, 2.0 mm
Vicat Softening Point 100 °C
@Load 1.02 kg
50°C per hour; ASTM D1525
Heat Distortion Temperature 192 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Lacqrene® 3351(AS) Impact Polystyrene
Overview of materials for Polystyrene, Heat Resistant Grade
Total PSI 4440(AS) High Impact Polystyrene

PTOTAL888 / 130613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.