MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Park Aerospace Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines and spaces and larger panel sizes.

Key Features and Benefits:

  • High thermal performance
  • Self adhesive bond to foam cores
  • Superior electrical properties
  • Typical Cyanate Ester processing
  • S-glass and Quartz options

Applications:

  • Fine-Line Multilayers
  • Backplanes
  • Surface-Mount Multilayers
  • BGA Multilayers
  • MCM-L's
  • Direct Chip Attach
  • Automotive
  • Underhood Automotive
  • Wireless Communcations
  • High Speed Computing
  • Radomes and Secondary Aerospace Structure

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.73 g/cc0.0625 lb/in³50% resin content
Water Absorption <= 0.050 %<= 0.050 %IPC-TM-650.2.6.2.1
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 20.7 GPa3000 ksiX; ASTM D3039
 20.7 GPa3000 ksiY; ASTM D3039
Poissons Ratio 0.140.14X; ASTM D3039
 0.140.14Y; ASTM D3039
Peel Strength 1.31 kN/m7.50 pli1 oz. Cu, at elevated temperature; IPC-TM-650.2.4.8.2a
 1.40 kN/m8.00 pli1 oz. Cu, after exposure to process solutions; IPC-TM-650.2.4.8
 1.40 kN/m8.00 pli1 oz. Cu, after solder float; IPC-TM-650.2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmC - 96/35/90; IPC-TM-650.2.5.17.1
 1.00e+13 ohm-cm1.00e+13 ohm-cmE - 24/125; IPC-TM-650.2.5.17.1
Surface Resistance 1.00e+13 ohm1.00e+13 ohmC - 96/35/90; IPC-TM-650.2.5.17.1
 1.00e+13 ohm1.00e+13 ohmE - 24/125; IPC-TM-650.2.5.17.1
Dielectric Constant  3.5
@Frequency 1e+10 Hz
3.5
@Frequency 1e+10 Hz
50% Resin Content; Stripline; IPC-TM-650.2.5.5.5
 3.6
@Frequency 1e+10 Hz
3.6
@Frequency 1e+10 Hz
50% Resin Content; Split Post Cavity
 3.6
@Frequency 2.50e+9 Hz
3.6
@Frequency 2.50e+9 Hz
50% Resin Content; Stripline; IPC-TM-650.2.5.5.5
 3.7
@Frequency 1e+9 Hz
3.7
@Frequency 1e+9 Hz
50% Resin Content; RF Impedance; IPC-TM-650.2.5.5.9
Dielectric Strength 65.0 kV/mm1650 kV/inIPC-TM-650.2.5.6.2
Dielectric Breakdown >= 50000 V>= 50000 VIPC-TM-650.2.5.6
Dissipation Factor  0.0070
@Frequency 1e+10 Hz
0.0070
@Frequency 1e+10 Hz
50% Resin Content; Split Post Cavity
 0.011
@Frequency 2.50e+9 Hz
0.011
@Frequency 2.50e+9 Hz
50% Resin Content; Stripline; IPC-TM-650.2.5.5.5
 0.011
@Frequency 1e+10 Hz
0.011
@Frequency 1e+10 Hz
50% Resin Content; Stripline; IPC-TM-650.2.5.5.5
Arc Resistance 160 sec160 secIPC-TM-650.2.5.1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 - 13.0 µm/m-°C
@Temperature -40.0 - 125 °C
6.11 - 7.22 µin/in-°F
@Temperature -40.0 - 257 °F
X/Y; IPC-TM-650.2.4.41
Glass Transition Temp, Tg 240 °C464 °FTMA; IPC-TM-650.2.4.24c
 250 °C482 °FDSC; IPC-TM-650.2.4.25c
 300 °C572 °FDMA (Tan d Peak); IPC-TM-650.2.4.24.3
Decomposition Temperature 376 °C709 °FTGA; 5% wt. loss; IPC-TM-650.2.4.24.6
 
Descriptive Properties
Methylene Chloride Resistance (% Weight Change)0.34IPC-TM-650.2.3.4.3
Pressure CookerPass60 min then solder dip @288°C until failure (max 10 min.); IPC-TM-650.2.6.16 (modified)
T260 (minutes)60+IPC-TM-650.2.4.24.1
T288 (minutes)30+IPC-TM-650.2.4.24.1
Z Axis Expansion (%)2.550-260°C; IPC-TM-650.2.4.41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 954-3 Curing Cyanate Resin
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Park Aerospace Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg
CRG Industries Advantic™ 30 Syntactic Foam
CRG Industries Advantic™ 40 Syntactic Foam

PPARK075 / 89347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.