MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 3325HRT PBT, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Celanex 3325HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at break.
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250°F (121°C) for 4 hours.
For subsequent storage of the material in the dryer until processed (<= 60 h) it is necessary to lower the temperature to 100° C.

Information provided by Celanese Corporation.

Key Words: 30% glass reinforced, copolyester, hydrolysis resistant, toughened
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.16 %0.16 %23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow 0.00 - 0.0050 cm/cm0.00 - 0.0050 in/inISO 294-4
 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psi5mm/min; ISO 527-2/1A
Elongation at Break 3.9 %3.9 %5mm/min; ISO 527-2/1A
Tensile Modulus 7.60 GPa1100 ksi1mm/min; ISO 527-2/1A
Flexural Strength 160 MPa23200 psiISO 178
Flexural Modulus 7.30 GPa1060 ksiISO 178
Izod Impact, Notched (ISO) 13.6 kJ/m²6.47 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eU
 4.60 J/cm²
@Temperature -30.0 °C
21.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.32 J/cm²6.28 ft-lb/in²ISO 179/1eA
 0.940 J/cm²
@Temperature -30.0 °C
4.47 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmIEC 60093
 1.30e+16 ohm-cm1.30e+16 ohm-cmASTM D257
Surface Resistance 8.60e+16 ohm8.60e+16 ohmASTM D257
 2.00e+17 ohm2.00e+17 ohmIEC 60093
Dielectric Constant  2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
IEC 60250
 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
ASTM D150
 3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 19.3 kV/mm489 kV/inshort term; ASTM D149
 32.0 kV/mm813 kV/inIEC 60243-1
Dissipation Factor  0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 122 sec122 secASTM D495
Comparative Tracking Index 375 V375 VIEC 60112
 573 V573 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C11.7 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 123 µm/m-°C68.3 µin/in-°FISO 11359-2
Melting Point 225 °C437 °FISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 206 °C403 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 184 °C363 °FISO 75-1, -2
Glass Transition Temp, Tg 19.0 °C66.2 °FISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 50.0 °C68.0 - 122 °Fhopper
 65.0 - 93.0 °C149 - 199 °Fcavity
Feed Temperature 230 - 245 °C446 - 473 °F
Zone 1 230 - 245 °C446 - 473 °F
Zone 2 240 - 250 °C464 - 482 °F
Zone 3 240 - 250 °C464 - 482 °F
Zone 4 245 - 260 °C473 - 500 °F
Die Temperature 250 - 260 °C482 - 500 °F
Melt Temperature 240 - 260 °C464 - 500 °F
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %Necessary low maximum
Hot-Working Temperature 250 - 260 °C482 - 500 °F
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergadur™ PB400 G30 UF UV Polybutylene Terephthalate (PBT)
BASF Ultraform® N 2200 G53 UNC Q600 25% Glass Filled POM
Celanese Celanex® 3225HRT PBT, 15% Fiberglass Reinforced
Celanese Celanex® 3209HRT PBT, 15% Fiberglass Reinforced
Celanese Celanex® 3314 PBT, 30% Glass Reinforced

PHCS062 / 123477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.