MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 3225HRT PBT, 15% Fiberglass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Celanex 3225HRT is a non-lubricated, 15% fiberglass reinforced Polybutylene Terphthalate copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at break.

Information provided by Celanese Corporation.

Key Words: 15% fiberglass reinforced, coplyester, hydrolysis resistant, toughened
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 69.0 MPa10000 psi50mm/min; ISO 527-2/1A
Elongation at Break 3.0 %3.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 3.882 GPa563.0 ksi1mm/min; ISO 527-2/1A
Flexural Strength 100.6 MPa14590 psiISO 178
Flexural Modulus 3.775 GPa547.5 ksiISO 178
Izod Impact, Notched (ISO) 5.80 kJ/m²2.76 ft-lb/in²ISO 180/1A
 5.70 kJ/m²
@Temperature 30.0 °C
2.71 ft-lb/in²
@Temperature 86.0 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  10.5 kJ/m²
@Temperature 30.0 °C
5.00 ft-lb/in²
@Temperature 86.0 °F
ISO 180/1U
 12.2 kJ/m²
@Temperature 23.0 °C
5.81 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 1.45 J/cm²6.90 ft-lb/in²ISO 179/1eU
 1.39 J/cm²
@Temperature -30.0 °C
6.61 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.570 J/cm²2.71 ft-lb/in²ISO 179/1eA
 0.620 J/cm²
@Temperature -30.0 °C
2.95 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 182 °C360 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 50.0 °C68.0 - 122 °Fhopper
 65.0 - 93.0 °C149 - 199 °Fcavity
Feed Temperature 230 - 240 °C446 - 464 °F
Zone 1 230 - 240 °C446 - 464 °F
Zone 2 235 - 250 °C455 - 482 °F
Zone 3 235 - 250 °C455 - 482 °F
Zone 4 240 - 260 °C464 - 500 °F
Die Temperature 250 - 260 °C482 - 500 °F
Melt Temperature 235 - 260 °C455 - 500 °F
Hot-Working Temperature 250 - 260 °C482 - 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 3210 Polyester (PBT), 20% Glass-Fiber
Celanese Celanex® 3325HRT PBT, 30% Glass Reinforced
Celanese Celanex® 3209HRT PBT, 15% Fiberglass Reinforced
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened

PHCS046 / 123461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.