MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1200-80A BLACK Ester-based Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes:


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.011 cm/cm
@Thickness 3.17 mm
0.0050 - 0.011 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 808010 sec; ASTM D2240
Hardness, Shore D 4242Instantaneous; ASTM D2240
Tensile Strength at Break 27.6 MPa
@Thickness 3.17 mm
4000 psi
@Thickness 0.125 in
Die C, 20 in/min (500 mm/min); ASTM D412
Elongation at Break 1100 %
@Thickness 3.17 mm
1100 %
@Thickness 0.125 in
Die C, 20 in/min (500 mm/min); ASTM D412
Tear Strength 96.4 kN/m550 pliDie C; ASTM D624
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 - 218 °C365 - 425 °F
Mold Temperature 37.8 - 60.0 °C100 - 140 °F
Drying Temperature 87.8 °C190 °F4 - 6 hrs
Moisture Content <= 0.020 %<= 0.020 %
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2700 S-80A FR Saturated Styrenic Block Copolymer, Flame Retardant - Non-PBDE/PBB
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade
Elkem (Bluestar Silicones) SILBIONE® LSR 4305 Liquid Silicone Rubber
Avient Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE)

PQZXA3619 / 59643

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.