MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Introduction: IROGRAN A 70 H 4673 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4673 M is part of the HUNTSMAN injection molding product range. It is processable at low temperatures and offers a specially designed, flexible material suitable for moldings.

Performance Features:

  • High transparency
  • Soft type
  • Good melt flow
  • Phthalate free
  • High elasticity
  • Easy coloring

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM D995
Melt Index of Compound 45 g/10 min
@Load 5.00 kg,
Temperature 190 °C
45 g/10 min
@Load 11.0 lb,
Temperature 374 °F
cm3/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7171ASTM D2240
Hardness, Shore D 2121ASTM D2240
Tensile Strength at Break 35.0 MPa5080 psiDIN 53504
Elongation at Break 880 %880 %DIN 53504
100% Modulus 3.40 MPa
@Strain 100 %
493 psi
@Strain 100 %
DIN 53504
300% Modulus 7.00 MPa
@Strain 300 %
1020 psi
@Strain 300 %
DIN 53504
Tear Strength 45.1 kN/m257 pliDIN 53515
Abrasion 3535[mm3]; ISO 4649
Compression Set  34 %
@Temperature 23.0 °C,
Time 252000 sec
34 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 48 %
@Temperature 70.0 °C,
Time 86400 sec
48 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Feed Temperature 175 °C347 °FInjection
Front Barrel Temperature 180 °C356 °FInjection
Adapter Temperature 180 °C356 °FInjection
Die Temperature 170 °C338 °FInjection
Melt Temperature 145 - 170 °C293 - 338 °F
 
Descriptive Properties
TMA High165°C
TMA Low120°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 95 K 4640 TPU-For Seals

PHU9907 / 150367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.